What is the salt spray test (ASTM B117)?
In the neutral salt spray test, samples are exposed to a salt water mist at a controlled temperature, and the time until red rust appears is measured. The test is used to compare materials and coatings; the hours are not the same as the service life in the field, but they reliably rank the resistance.
ER-Bİ grades and salt spray hours
| Grade | Material | Salt spray |
|---|---|---|
| W1 | Zinc-plated steel | 72–100 hours (by product) |
| W2 | 430 stainless band and housing, plated screw | Band 400 hours |
| W4 | 304 stainless (band, housing, screw) | 800 hours |
| W5 | 316 stainless | At least 2,500 hours |
The hours for each product are in the materials table on its page.
What accelerates corrosion
- Chloride: sea air, road salt and pool environments accelerate rusting; choose W5.
- Moisture and condensation: use W2 or W4 for connections that stay wet.
- Contact between different metals: choose clamp and fasteners of the same grade to avoid galvanic corrosion.
- Coating damage: on W1 clamps, coating scratched during assembly can start corrosion.
Choosing by environment
- Dry indoors → W1
- Humid, semi-outdoor → W2
- Outdoors, food, chemicals, engine compartment → W4
- Marine, salt, chloride → W5
For details of the grades see the W1–W5 material grades guide.